根据(1-x)NBT-xBaTiO3的配方,分别选取不同组成点,采取不同的预合成温度,根据样品的体积密度和压电性能,确定最佳的预烧温度。
According to the samples of (1 - x) NBT- xBaTiO3, various compositions and different precalcination temperature were chosen and adoped respectively. The best calcination temperature was determined by measuring the volume density and piezoelectric properties of the samples.