液态树脂在管道修复中的应用
摘要
介绍了液态树脂修复材料的特性,以及管道修复程序,包括去除旧涂层,呆用高压水冲洗技术设备对管道进行必要的维修或更换、表面处理准备等工作程序,并结合液态树脂修复材料在美国和哈萨克斯坦等国的应用实例,说明了该涂料的显著特点。
出处
《油气储运》
CAS
北大核心
2005年第B12期115-118,共4页
Oil & Gas Storage and Transportation
参考文献7
-
1Taylor S A.Field Removal of Cold-Applied Tape systems from Large Diameter Transmission Lines Using High and Ultra High Pressure Water Jetting, Paper No. 01605, Corrosion 2001,( Houston, TX: NACE).
-
2Denney A K, S I Coleman et al.Products Pipeline Rehabilitated While on Stream, Oil and Gas Journal, January 9, 1995.
-
3SSPC-SP 1, Cleaning of Uncoated Steel or a Previously Coated Surface Prior to Painting or Using Other Surface Preparation Methods, (Pittsburgh, PA: SSPC).
-
4NACE No. 2/SSPC-SP 10 Near-White Metal Blast Cleaning, (Houston, TX: NACE, 1994).
-
5Fauntleroy T, Kehr A.Fusion Bonded Epoxy Application Manual, 3M publication, August 1990.
-
6Snyder G, Bleuthin L.Abrasive Selection: Performance and Quality Considerations, JPCL, Vol. 6, No. 3, March 1989,pp. 46-53.
-
7Blasting Using Compressed Air Equipment, Wheelabrator Abrasives, Inc., ABC3886-5/97 May 1997, W Derden, "One-Pass Pipeline Rehabilitation," Pipeline and Utilities Construction, July 1991.
-
1用液态树脂补换并稳固混凝土板[J].市政工程国外动态,2003(2):17-19.
-
2宋长安.压力容器焊缝缺陷的修复[J].本钢技术,1990(4):29-32.
-
3石金磊,陈伟杰.手工电弧焊管道修复技术应用[J].中国新技术新产品,2010(16):117-118. 被引量:4
-
4专利介绍[J].中国胶粘剂,2008,17(12):63-64.
-
5张淑洁(译),王瑞(校).现存排污管和管道修复用聚氯乙烯管线衬里和水泥薄浆的安装规程[J].非开挖技术,2006(4):49-52.
-
6陈葆琦.液化石油气贮罐高应力裂纹的产生原因及裂纹修复[J].焊接技术,1993,22(5):35-37.
-
7谢江,侯志强,吕一仕,王淦刚,赵建仓,赵明凯.超(超)临界机组P92钢厚壁管道修复的焊接工艺设计[J].焊接,2014(12):48-51.
-
8刘学谦,高明,杨爱萍,陈喆.液化石油气储罐高应力裂纹的产生和修复[J].天津燃气,2005(4):11-14.
-
9李捷,倪振航.中板工作辊堆焊修复材料的优化[J].机械工人(热加工),2006,30(9):49-50.
-
10王若愚.管道修复的一种非常规焊接方法[J].焊接,2009(1):60-63. 被引量:1