用含Hf的中间层合金钎接或暂存液相连接单晶高温合金时,为了使Hf尽快地由焊缝区向母体合金扩散,研究了Hf在基体相Ni(γ)和Ni3AI(γ′)中的扩散行为,并算出扩散系数和扩散激活能,找到了扩散系数与温度、浓度的关系。
The Hf-containing alloy was selected as a interlayer for brazing and Transient-Liquid-Phase(TLP) bonding of single crystal superalloy, in which element Hf should diffuse as quickly as possible from bond to matrix phase. The objective of this investigation is to determine the diffusion behaviour of Hf in two matrix phases of superalloy,the Ni-rich solid solution(y)and intermetallic compound(Ni3Al). In present work,the diffusion coefficient, diffusion activity energy in two matrix phases, and their relation with temperature and Hfcontent are reported, which are useful to select a proper bonding condition.