摘要
In this paper, samples of CaO-riched MgO-CaO added with Y2O3 were prepared and the growth rate of MgO grains were investigated, and the calculation of the grain growth active energy at different temperatures was done for the high performance anti-hydration CaO-riched MgO-CaO clinker. It is of significance for decreasing the synthetic temperature in industry production.
In this paper, samples of CaO-riched MgO-CaO added with Y2O3 were prepared and the growth rate of MgO grains were investigated, and the calculation of the grain growth active energy at different temperatures was done for the high performance anti-hydration CaO-riched MgO-CaO clinker. It is of significance for decreasing the synthetic temperature in industry production.