摘要
莱钢炼钢厂采用轻烧镁块代替白云石进行造渣,使炉渣中(MgO)稳定在9%-10%,比用轻烧白云石炉渣(MgO)含量提高了2%-3%左右,满足溅渣工艺要求,提高了溅渣护炉效果,有极大的推广价值。
The steel-making plant of Laiwu Steel Corporation used caustic-burned Magnesite lump to slag replaced with the caustic-burned dolomite, which stabilize the percent of MgO in slag with 9% - 10%. This may increase the MgO percent with 2% - 3% than that in dolomite. This can meet the process of slag splashing to protect the converter, make a rapid progress in slag splashing and can be popularized.
出处
《莱钢科技》
2006年第3期38-39,共2页
Laigang Science & Technology
关键词
轻烧镁块
溅渣护炉
caustic-burned magnesite lump, slag splashing to protect the converter