期刊文献+

焊趾部位缺欠的超声检测及分析

UT Inspection and Indication Analysis on Weld Toe
下载PDF
导出
摘要 详细介绍了双面螺旋埋弧焊焊趾部位缺欠的超声检测工艺和方法,通过金相分析验证了其有效性。分析了焊趾部位缺欠对焊缝力学性能的影响及焊趾部位缺欠产生的原因。为了我国油气输送管网建设的百年大计,提出应通过订货附加技术条件来弥补现行的焊趾部位缺欠超声波验收标准的不足。 It introduces clearly UT inspection procedure and methods on submerged arc weld toes indication,and also its effectiveness is verified with micro-metal analysis.Also it analysis weld toes indication causes and weld toes indication influence on mechanical property.In order to national oil-gas pipelines plan,it also raises the shortage of practical Standards and also states the measurement to revise the standards to UT inspection on weld toes in technical requirements.
作者 胡剑
出处 《焊管》 2006年第4期80-83,共4页 Welded Pipe and Tube
关键词 双面螺旋埋弧焊管 焊趾 焊趾缺欠 超声检测 SSAW weld toe weld toe defect UT
  • 相关文献

参考文献3

  • 1BLITY J,SIMPSON G.Ultrasonic Methods of NDT[M].[s.l.]:Chapman & Hall,1996.
  • 22000 Annual Book of ASTM Standards[S].
  • 3李家伟,陈积懋.无损检测手册[M].北京:机械工业出版社,2004.

共引文献27

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部