摘要 采用三种不同水泥用量的混凝土试样置放于酸性河道旁侧并在大气曝露之后,对混凝土试样进行检测与分析。通过观察与检测,混凝土被确认有一定程度的劣化现象。试验结果表明,混凝土的劣化深度和脱落深度随时间推移有明显的增加,变化量在0.7mm/年~1.3mm/年之间。 Concrete test sample of three joint material dosage is placed near an acid river, air exposure is carried out, the character of test sample is measured, and a change situation is analyzed. By the observation and measurement,degradation of test sample was boiled to some extent and accepted. Considering the examination result, the deterioration depth and omission depth of concrete have a remarkable increase in connection with the age, and the amounts of change are 0.7 mm/yr, and 1.3 mm/yr, respectivdy.
出处 《山西建筑》 2006年第15期137-138,共2页 Shanxi Architecture
关键词 混凝土 压缩强度 劣化深度 脱落深度 concrete, compression strength, deterioration depth, falling-off depth
  • 相关文献

参考文献3

  • 1Sidney Mindess,J.Francis Young.混凝土[M].方秋清,译.北京:中国建筑工业出版社,1989.10.
  • 2V. Pavlik, Corrosion of Hardened Cement Paste by Acetic and Nitric Acids Part Ⅱ : Formation and Chemical Composition of the Corrosion Products Layer [ J ]. Cement and Concrete research,Vol. 24, No. 8, 1994, pp. 1 495-1 508.
  • 3R. I. Gilbert, Time effects in Concrete Structures [ J ]. Elesivier Science Publisher B. V, 1988(2) :87-88.

共引文献2

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部