摘要
研究了Co及Co-10Ce合金在900℃空气中的热腐蚀行为;并对Co-10Ce合金的腐蚀机制进行分析。在高温情况下腐蚀24 h后,可以得到,Co-10Ce合金的晶粒比纯Co小,并且腐蚀到基体的深度要比纯Co少。
The hot corrosion behavior of Co and Co - 10Ce alloy was studied in air at 900℃ ,and the corrosion mechanism of Co - 10Ce alloy was analyzed. After 24 hours, it could be found that the grain size and the corrosion depth of Co - 10Ce were smaller than those of pure Co.
出处
《辽宁化工》
CAS
2006年第8期439-441,共3页
Liaoning Chemical Industry