摘要
分析造成Z4/H烟草真空回潮机抽真空装置腐蚀的原因,据此进行了技术改进。改造后腐蚀周期从1年延长到8年以上。
The reasons of corrosion of the vacuum system of 241H tobacco vacuum conditioner were analyzed, and technical improvement was made to prevent vacuum system from quick corrosion. The ocuurence of corrosion of the system could be delayed from one year to more them 8 years after improvement.
出处
《腐蚀与防护》
CAS
北大核心
2006年第8期426-427,共2页
Corrosion & Protection
关键词
真空装置
真空回潮机
腐蚀
酸性
不锈钢
改进
Vacuum system
Vacuum conditioner
Corrosion
Acidity
Stainless steel
Improvement