摘要
本文通过对典型正交玻璃钢板材的45°方向和0°方向进行拉伸试验,从性能数据和材料破坏过程及现象两个方面进行对比分析,对正交板材两个方向性能指标的显著差异和破坏过程以及破坏现象进行了总结。提醒结构设计中值得引起注意的一些细节。
Here, through tension tests of 45° specimens and 0° specimens oforthotropic FRP plate, the author studied and compared the difference of mechanical properties and testing appearance between them. Then the author hopes this paper could help FRP designers to put sufficient highlight on the corresponding spot.
出处
《玻璃钢》
2006年第4期17-20,共4页
Fiber Reinforced Plastics
关键词
45°板
0°板
拉伸性能
对比
45° specimens
0° specimens
tension property
comparison