摘要
何家岩原生金矿石中,金及金的载体矿物粒度微细,采用常规氰化浸出,金浸出率仅23%左右。对浮选金精矿采用细菌预氧化—氰化浸出工艺,金浸出率可达到92.73%。因此,采用浮选—浮选金精矿细菌预氧化—氰化浸出是处理该矿石较为适宜的工艺。
In Hejiayan primary gold ores,the particle size of gold and gold carrier minerals is microfine. If the conventional cyanide leaching is adopted, the leaching rate of gold is about 23%. However, when the technology of bacterial pre - oxidation and cyanide leaching for flotation concentrate of gold is used, the leaching rate of 92.73 % is reached. The experimental results proved that the bacterial pre-oxidation and cyanide leaching technology is suitable for processing of Hejiayan gole ores.
出处
《矿产综合利用》
CAS
2007年第2期3-6,共4页
Multipurpose Utilization of Mineral Resources
关键词
细粒原生矿
浮选
细菌预氧化
氰化浸出
Microfine-grained primary gold ore
Flotation
Bacterial pre-oxidation
Cyanide leaching