摘要 通过对热轧窄钢带合格产品、检验废品、中间轧废品的关系进行多元线性回归统计分析,认为检废和中间轧废的增加,使得合格率减小,产生检废主要原因是拉窄、超宽、超厚、卷取废,产生中间轧废主要原因是坯料劈头、坯料加热质量不好、调整不当以及机械、电气事故,提出了减少检废和中间轧废的技术措施。 The paper analyses the relationship of the yield rate, the rejected rate and the mid - rolling defective index with multivariate linear regression method. The conclusion shows that the yield ratio decreases when the rejected ratio and the mid - rolling defective index increase. The rejected causes are that the product is narrow, superwide, superthiek, rejected during the rolling process. The mid - rolling defects are because of the blank craze, caused by improper heating system and adjustment method, mechanical and electric accidents. It puts forward the technical countermeasures.
作者 袁琨
出处 《包钢科技》 2007年第2期17-19,共3页 Science & Technology of Baotou Steel
关键词 热轧 窄钢带 合格率 hot roiling narrow strip yield ratio
  • 相关文献

参考文献2

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部