摘要
针对青海某大型钼矿床矿石进行了选矿试验研究。采用一次粗选、两次扫选、三次精选闭路流程取得了精矿含钼51.68%、钼回收率96.40%的技术指标。该工艺流程合理,易于工业化。
Mineral processing experiment and study have been carried out for the ores in a certain large molybdenum deposit from Qinghai. By adopting the closed circuit flotation flowsheet of single - stage roughing, two - stage scavenging and three - stage cleaning, a concentrate of 51.68 % Mo was obtained with a recovery of 96.40%. This flowsheet is simple and easy to be industrialized.
出处
《矿产保护与利用》
2007年第2期31-33,共3页
Conservation and Utilization of Mineral Resources
关键词
辉钼矿石
浮选
回收
流程
molybdenite ore
floatation
recovery
flowsheet