阐述了5052合金铸轧坯料生产时冷隔缺陷产生的机理,结合超型FATA—HUNTERΦ1003×1850mm机多年的生产实践经验,提出了消除铸轧冷隔缺陷的措施。
The forming mechanism of cold shut defect on 5052 alloy stock during the casting was described. Combining with practical experience on FATA- HUNTER Φ1003×1850mm cast -rolling mill, the measures to eliminate cold shut were put forward.