1Congqin NING,Qingchang .MENG and Yu ZHOU School of Materials Science and Engineering, Harbin institute of Technology, Harbin 150001, China Haitao LIU Department of Chemical Engineering, Qiqihar Institute of Light Industry, Qiqihar IG1006. China.Microstructure of Bioglass/Hydroxynpatite Coatings on Ti Substrate[J].Journal of Materials Science & Technology,2001,17(1):35-36. 被引量:3
2Yu Yaoting(俞耀庭) Zhang Xingdong(张兴栋).Biomedical Materials(生物医用材料)[M].Tianjin:Tianjin University Press,2000.131.
3Fu Tao(付涛) Huang Ping(黄平) Han Yong(憨勇) Xu Kewei(徐可为).Rare Metal Materials and Engineering(稀有金属材料与工程),2000,29(3):168-168.
4Zhang Yumei(张玉梅) et al.Rare Metal Materials and Engineering(稀有金属材料与工程),1999,28(2):125-125.
1LONG M, RACK H J. Titanium alloys in total joint replacement -A materials science perspective [J]. Biomaterials, 1998, 19(18): 1621-1639.
2LIU X Y, CHU P K, DING C X. Surface modification of titanium, titanium alloys, and related materials for biomedical applications [J]. Materials Science and Engineering: R: Reports, 2004,47(3/4): 49-121.
3GEETHA M, SINGH A K, ASOKAMANI R, et al. Ti based biomaterials, the ultimate choice for orthopaedic impiants-A review [J]. Progress in Materials Science, 2009, 54(3): 397-425.
4KOKUBO T. Titanium-based bone-bonding composites having inverted concentration gradients of alkali and titanium ions in a surface layer: U.S., 5609633[P]. 1997-05-11.
5WANG Q, GUO Z H, CHUNG J S. Formation and structural characterization of potassium titanates and the potassium ion exchange property [J]. Materials Research Bulletin, 2009, 44(10): 1973-1977.
6VIANA B C, FERREIRA 0 P, SOUZA-FILHO A G, et al. Alkali metal intercalated titanate nanotubes: A vibrational spectroscopy study [J]. Vibrational Spectroscopy, 2011, 55(2): 183-187.
7CHANG H, HUANG P J. Thermo-Raman studies on anatase and rutile [J]. Journal of Raman spectroscopy, 1998,29(2): 97-102.
8NAUMKIN A V, KRAUT-V ASS A, GAARENSTROOM S W, et al. NIST X-ray Photoelectron Spectroscopy Database 20, Version 4.1.
9ALKHATEEB E, VIRTANEN S. Influence of surface self- modification in Ringer's solution on the passive behavior of titanium [J]. Journal of Biomedical Materials Research, 2005, 75A (4): 934-940.
10BAI Y, HAO Y L, LI S J, et al. Corrosion behavior of biomedical Ti-24Nb-4Zr-8Sn alloy in different simulated body solutions [J]. Materials Science and Engineering: C, 2013, 33(4): 2159-2167.