摘要
阐述了短绒产生的原因与危害,分析了清梳联短绒增加较多的原因,提出了清梳联工序有效控制短绒的措施,认为应采取"连续喂棉、薄喂轻打"措施,减少纤维损伤;同时注意开松梳理适度,排除结杂和减少短绒兼顾。
In this paper the procreant cause and imperil of short fibers are expounded with the cause of short fibers increasing in blowing-carding unit analyzed and effective measures to control short fibers put forward. The measure "to feed cotton in continuous way with less feeding and light beating" should be adopted to reduce the fiber damage in addition to a suitable opening and carding being maintained which removes impurities and reduces short fibers.