介绍了低游离甲醛含量的低醛/尿摩尔比脲醛树脂木材粘合剂的生产新方法。利用控制不同反应阶段不同工艺条件,使整个生产周期缩短20%,并充分利用反应热,使能耗降低。
A new method was introduced in this paper, which was used to produce low molar ratio ureaformaldehyde adhesive resin as a wool adhesive of low free fomcaldehyde conetent. By using different conditions in different reactive periods, the reactive cycle reduced 20 %. The energy consume decreased by making good use of the reactive heat
出处
《广州化工》
CAS
2007年第3期8-10,共3页
GuangZhou Chemical Industry
关键词
脲醛树脂粘合剂
绿色节能
游离甲醛
生产
urea-formaldehyde resin adhesive
green energy-saving
free fomcaldehyde
production