摘要
通过对宁夏小尾寒羊毛的物理性能、电学性能、机械性能、化学性能和染色性能的系统测试分析,认为小尾寒羊毛品质支数接近48~56s,但粗腔毛含量较高,今后改良的重点应放在降低粗腔毛含量上。建议在没有改良成功前不应盲目建立小尾寒羊毛基地。
Through to Ningxia Small-tail-cold wool physical performance, the electricity performance, the machine capability, chemistry per- formance and the dyeing performance system test analysis, thought the Small--tail--cold wool approaches a 48-56^s wool, but the thick cavity wool content is higher, the next improvement will be supposed to put with emphasis in reduces in the thick cavity wool content. Suggested in has not improved successi'ully before should not blindly establish the Small--tail--cold wool base.