摘要
介绍了一、二次球磨作业10:3工艺在某选矿厂一选车间的应用,结果表明:使用该工艺后,重选作业-200目给矿粒度质量分数提高5%-10%,重精品住提高0.36%,重尾品位降低2.19%。
Application of 10 : 3 process on primary and secondary ball grinder at No.1 sparation workshop of a concentrator was introduced. The applicated results indicated that mass fraction of minus 0.074 mm feeding mine granularity was increased 5%~10%, gravity concentrate extract mine grade was increasd 0.36%, graity concentrate tailing mine grade was decreased 2.19% after appling 10 : 3 technique.
出处
《山西冶金》
CAS
2007年第3期53-54,共2页
Shanxi Metallurgy
关键词
10:3工艺
给矿粒度
重选作业
10:3 process
feeding mine granularity
gravity concentration