期刊文献+

负极集流体铜箔对锂离子电池的影响 被引量:20

EFFECTS OF COPPER FOIL AS CATHODE CURRENT COLLECTOR ON PERFORMANCE OF LI-ION BATTERIES
下载PDF
导出
摘要 用循环伏安、扫描电子显微镜和循环检测装置研究了表面状况不同的铜箔集流体对锂离子电池性能的影响.结果表明,电解液在毛面铜箔表面发生还原反应的程度比在光面铜箔表面显著,其阳极溶解电位比光面铜箔约低0.8 V,且溶解需要的能量较少,相对耐腐蚀性较差.光面铜箔集流体锂离子电池的容量循环衰减要比毛面铜箔小,且随着循环的进行,后者的容量衰减趋势明显加剧. The effects of copper foils with different surface profile as current collector on performance of Li-ion battery are investigated by cyclic voltammetry measurements, scanning electronic microscopy observations as well as measurement of of cyclic performance of batteries. The results indicate that the reducing reaction of electrolyte on the foil with rough surface is much visible than on that with shiny surface, the dissolution potential of matte copper foil is 0. 8 V lower than that of the shiny copper foil which implies that the reduction reaction on the rough foil needs much less energy. In other wards, the rough foil is less corrosion resistant. The capacity decrease of battery Li-ion batteries is much smaller than that with with shiny copper foil as cathode current collector for matte copper foil, and the capacity decrease for the latter becomes much obviously speedy by cycling.
出处 《腐蚀科学与防护技术》 CAS CSCD 北大核心 2007年第4期265-268,共4页 Corrosion Science and Protection Technology
关键词 锂离子电池 毛面铜箔 光面铜箔 Li-ion battery matte copper foil shiny copper foil
  • 相关文献

参考文献10

  • 1张世超,蒋涛,白致铭.电解铜箔材料中晶面择优取向[J].北京航空航天大学学报,2004,30(10):1008-1012. 被引量:20
  • 2Clouser.Electrodepesited copper foil[P],1995,美国专利:USP5:454-926.
  • 3Lu L,Li S X,Lu K.An abnormal strain rate efect on tensile behavior in nanecrystalline copper[J].Scripta Materialia,2001,45:1163.
  • 4Ota H,Kominato A,Chun W J,et al.Effect of cyclic phosphate additive in non-flammable electrolyte[J].J.Power Sources,2003,119-121:393.
  • 5Shin J S,Han C H,Jung U H,et al.Effect of Li2CO3 additive on gas generation in lithium-ion batteries[J].J.Power Sources,2002,109:47.
  • 6Abe K,Yoshitake H,Kitakura T,et al.Additives-containing functional electrolytes for suppressing electrolyte decomposition in lithium -ion batteries[J].Electrochim.Acta,2004,49:4613.
  • 7黄可龙,吕正中,刘素琴.锂离子电池容量损失原因分析[J].电池,2001,31(3):142-145. 被引量:32
  • 8Tobishima S,Takei K,Sakurai Y,et al.Lithium ion cell safety[J].J Power Sources,2000,90(2):188.
  • 9Spotnitz R,Franklin J.Abuse behavior of high-power,lithiumion cells[J].J.Power Sources,2003,113:81.
  • 10Zhao M Ch,Dewald H,Staniewicz R J.Quantitation of the dissolution of the graphite-coated copper foil in lithium-ion battery electrolytes by flame atomic absorption spectroscopy[J].Electrochim.Acta,2004,49:677.

二级参考文献16

  • 1[1]Lu L,Li S X ,Lu K.An abnormal strain rate effect on tensile behavior in nanocrystalline copper [J].Scripta Materialia,2001,45:1163~1169
  • 2[2]Wang Y M,Wang K,Pan K,et al.Microsample tensile testing of nanocrystalline copper[J].Scripta Materialia,2003,48:1581~1586
  • 3[3]Ma E.Instabilities and ductility of nanocrystalline and ultrafine-frained metals [J].Scripta Materialia,2003,49:663~668
  • 4[4]Sanders P G,Youngdahl C J,Weertman J R.The strength of nanocrystalline metals with and without flaws [J].Materials Science and Engineering,1997,A234~236:77~82
  • 5[5]Valiev R Z.Structure and mechanical properties of ultrafine-grained metals[J].Materials and Engineering,1997,A234-236:59~66
  • 6[6]Song H W, Guo S R.A coherent polycrystal model for the inverse hall-petch relation in nanocrystalline metals[J].Nanostructured Materials,1999,11(2):203~210
  • 7[7]Kim H S, Estrin Y, Mark B, et al.Constitutive modeling of strength and plasticity of nanocrystalline metallic materials[J].Materials Science and Engineering,2001,A316:195~199
  • 8[8]Wang Ning, Wang Zhirui,Aust K T,et al.Effect of grain size on mechanical properties of nanocrystalline materials[J].Acta Metal Mater,1995,43(2):519~528
  • 9[9]Clouser.Electrodeposited copper foil [P].USP5,454,926,1995
  • 10[10]Prengaman.Electrowinning anode [P].USP6,131,798,2000

共引文献50

同被引文献176

引证文献20

二级引证文献83

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部