摘要
硝化棉100~150,丙烯酸酯250~350份,水2000份,乳化剂适量,催化剂适量,在50~60℃下接枝共聚4~6小时。反应产物切割、干燥。干燥物120份,混合溶剂880份,常温下搅拌溶解既为成品。本品适用于各种皮革及人造革的顶层涂饰。图2,表4。
Nitrocellulose 100~150, acrylate 25~350, water 2000 parts, suitable amounts of emulsifier and catalyst are graft-copolymerized at 50-60 ℃ for 4~6 hours. The reaction products are then cut and dried. Thus, the dried products 120 are mixed with solvents 880 parts and, by stirring at a normal temperature, dissolved to give finished products. This product is suitable for the top coatings of all leathers and artificial leathers.