摘要
应用刷涂-热氧化法,在不同热氧化温度(分别为400℃、440℃、470℃)下制备Ru、Ir、Ti三元金属氧化物电极。通过电化学性能、强化寿命以及电极形貌分析得出:440℃热氧化温度下制备的Ru0.15Ir0.15Ti0.7/Ti电极析氯电位低、催化活性强、强化寿命长;且该温度下的反应电阻也最小。
A kind of metal oxide anode is prepared through brush-thermal oxidation at 400℃ ,440℃,470℃ . Influence of thermal temperature on electrode electrochemistry performance and surface morphology is investigated. The results of electrode electrochemistry performance and accelerated life tests indicate that Ru0.15Ir0.15Ti0.7/Ti electrode has low chlorine potential, excellent catalyze selectivity, long internsifying life and low reaction resistance when the thermal treatment temperature is 440℃.
出处
《材料开发与应用》
CAS
2007年第4期4-6,26,共4页
Development and Application of Materials
关键词
金属氧化物电极
热氧化温度
催化活性
交流阻抗
Metal oxide anodes
Thermal oxidation temperature
Catalyze character
Electrochemical impedance spectroscopy (EIS)