TMCP钢E40-Z35厚钢板低温CTOD韧性试验 被引量:6

LOW Temperature CTOD Toughness Test for E40-Z35 Heavy Plate Produced by TMCP
下载PDF
导出
摘要 对新研发的TMCP钢E40-Z35厚钢板进行了低温CTOD试验,结果表明其具有良好的低温韧性。讨论了TMCP钢国际船级社认证中进行CTOD试验的相关问题:包括试验规范的选择、试验温度的确定和试验结果的评价等,同时介绍了CTOD的概念、试验方法、试验过程及其检验试验结果有效性的方法。 The low temperature (--20℃) CTOD (Crack Tip Opening Displacement) test for E40-Z35 heavy plate produced by TMCP (Thermo-mechanical Control Process) is performed. The results show that the E40- Z35 steel possesses excellen'e toughness in low temperature. The problems about CTOD test during international classifying have been discussed, including the choice of test standards, the determination of test temperature and the assessment of test results and so on. The concept of CTOD, the method of CTOD test, the procedure of CTOD test and the approach of inspecting the validity of test results are all presented in the paper.
出处 《轧钢》 2007年第4期1-4,共4页 Steel Rolling
关键词 TMCP钢 厚钢板 CTOD试验 低温韧性 TMCP heavy plate CTOD test low temperature toughness
  • 相关文献

参考文献8

  • 1GB/T2358-1994.金属材料裂纹尖端张开位移试验方法[S].[S].,..
  • 2中国船级社.材料与焊接规范[S].北京:人民交通出版社,2006.
  • 3GB712-2000.船体用结构钢[S].
  • 4Norsk Standard NS-EN 10225-2001,Weldable Structural Steels for Offshore Structures-Technical Delivery Conditions[S].
  • 5British Standard Institution.BS7448:Part1:1991.Method for Determination of KIC、 Critical CTOD and Critical J Values of Metallic Materials[S].
  • 6Takahiro KAMO,Takeshi URABE,Kazushi OHNISHI.Development of 550MPa Yield Strength Steel Plate for Offshore Structures[A].Proceedings of OMAE04 23rd International Conference on Offshore Mechanics and Arctic Engineering,June20-25,2004[C].Vancouver,British Columbia,Canada.
  • 7苗张木,陶德馨,杨荣英,李永信.焊接接头韧度CTOD评定的适用性与允许值研究[J].机械强度,2006,28(1):150-154. 被引量:22
  • 8苗张木,王振宇.厚钢板焊接接头韧性CTOD试验评定技术及应用[J].宽厚板,2006,12(6):23-28. 被引量:13

二级参考文献37

共引文献44

同被引文献72

引证文献6

二级引证文献20

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部