摘要 马氏体不锈钢1Cr17Ni2银亮材在切削加工过程中易产生影响使用的积屑瘤缺陷,影响产品质量。通过对产生缺陷原因的分析和生产实践,找到一条通过合理坯料与成品规格合理匹配、控制切削三要素解决1Cr17Ni2银亮材表面积屑瘤、翻皮缺陷的途径。 The silver bright material of martensitic stainless steel 1Cr17Ni2 was easy to cause the built - up edge during the cutting process, which influences the product quality. Through the analysis of reasons for defects and production practice, a way was found that solved the surface built - up edge of 1Cr17Ni2 silver bright material and skull patch by reasonable matching of blank and product size as well as controlling of three factors of cutting.
作者 肖彬
出处 《特钢技术》 CAS 2007年第3期34-35,54,共3页 Special Steel Technology
关键词 马氏体 1CR17NI2 积屑瘤 切削三要素 Martensite, 1Cr17Ni2, Built- up edge, Three factors of cutting