摘要
通过改进排气眼,改进浇注工艺,提高型砂性能等措施,较好地解决了气缸体铸件气孔缺陷,使气孔废品率由原来的5%以上降到1.5%以下,取得了较好的效果。
By adopting measures such as changing the vent shape, improving pouring process and reducing gas generation of resin sand and so on, the blow hole defect problem of the cylinder block has been quite successfully solved, and the blowhole rejection rate was reduced from more than 5% to less than 1.5%.
出处
《现代铸铁》
CAS
2007年第5期17-18,共2页
Modern Cast Iron
关键词
气缸体铸件
气孔缺陷
工艺改进
cylinder block casting
blowhole defect
process improvement