摘要
测定了1600℃下用不同还原剂处理上钢三厂转炉渣时渣中FeO的还原动力学曲线。研究了用C及煤矸石作还原剂时,渣中FeO和P2O5的变化关系,确定了还原后转炉渣直接作水泥熟料的最佳条件。
Several sorts of reductive agent were used to treat the converter slag of Shanghai No.3 Steel Work and the reductive kenitic curves of FeO at 1600℃ were measured.Taken carbon and gangue as reductive agent,the relationship of FeO and P 2O 5 in slag were determined.The optimum process reducing converter slag into cement clinker is proposed.
出处
《环境工程》
CAS
CSCD
北大核心
1997年第3期54-57,共4页
Environmental Engineering