莱钢2^#1880m^3高炉通过煤比的提升将矿批逐渐扩大至50t/p。大矿批操作保证了高炉的长期稳定顺行,入炉焦比达到380kg/t,煤比140kg/t,利用系数达到了2.6t/(m^3·d)。
Abstract: Through enhancing the coal ratio, Laigang 1880 -m^3 blast furnace #2 gradually expanded ore weight to 50 t/p, which ensured its steady and smooth operation. With its charge coke ratio reaching 380 kg/t,coal ratio 140 kg/t and utilization factor up to 2.6 t/(m^3 · d).
出处
《莱钢科技》
2007年第6期9-10,共2页
Laigang Science & Technology
关键词
大矿批
高炉
粒煤喷吹
Large-batch ore
B.F.
granular coal
injection