摘要
本文将煤焦与KOH混合,在Ar气流中进行低温、高温二次热处理,制得了比表面积为2918m2/g的活性炭。考查了操作条件对产品性能的影响。
The activated carbon of surface area of 2918m 2/g was made in this paper through a low and a high temperature heat treatments of the mixture of KOH and coal char under Ar flow The main factors that influence the properties of the activated carbon was investigated The produced activated carbon was analysed with Xray diffraction
出处
《燃料化学学报》
EI
CAS
CSCD
北大核心
1997年第3期253-257,共5页
Journal of Fuel Chemistry and Technology