摘要
利用扫描电镜在位拉伸方法(ISL-SEM),研究了毛竹/杉木层积复合材在受到外力作用下3点弯曲和剪切破坏的微观形变过程;结合扫描电镜所观测的形貌图,分析了该情况下层积材的典型破坏规律;总结了气干和水湿处理后,竹杉层积复合材剪切破坏模式以及气干条件下弯曲破坏模式。
The micro-failure process of three-point bending and shearing strength on Moso bamboo-Chinese fir laminated composites under loading was investigated by the in-situ linear-scan electron microscope method (ISL-SEM). The typical failure regularities were analyzed in accordance with the images observed by scanning electron microscope. The breakage patterns of Moso bamboo-Chinese fir laminated composites, including shearing failure after air-dry and water soaking and bending failure under air-dry condition, were also summarized.
出处
《东北林业大学学报》
CAS
CSCD
北大核心
2008年第2期27-29,共3页
Journal of Northeast Forestry University
基金
国家“十一五”支撑项目(2006BAD19B07)
国家林业局“948”引进项目(2003-4-27)
关键词
毛竹杉木层积材
扫描电镜在位拉伸
弯曲
剪切
破坏模式
Moso bamboo-Chinese fir laminated composites
In-situ linear-scan electron microscope
Bending
Shearing