摘要
为了给57%钼精矿工艺技术研究项目提供先进合理的工艺流程,项目组进行了室内试验研究。研究结果表明,粗精矿采用浓缩脱药,经过一段再磨、一次或两次擦洗、多次精选的工艺流程,即可全部生产出57%钼精矿,精选回收率达到97%。
In order to the project provides the advanced reasonable technical process to 57% molybdenum ore concentrate processing technology research, the project group carried on in the room the experimental study,the findings had indicated that. The thick ore concentrate uses the concentration to escape the medicine, passes through a section to regrind the technical process which,one or two times scours,selects many times,then completely produces 57% molybdenum ore concentrate,the selection returns-ratio achieves 97%.
出处
《有色金属(选矿部分)》
CAS
2008年第1期23-25,共3页
Nonferrous Metals(Mineral Processing Section)
关键词
粗精矿
浓缩脱药
擦洗
再磨
thick ore concentrate
the concentration escapes the medicine
scouring
regrinding