PPS/GF/Nano-CaCO3三元复合材料的结晶性能 被引量:2

Crystallization Properties of PPS/GF/Nano-CaCO_3 Ternary Composites
下载PDF
导出
摘要 研究了纳米级碳酸钙(Nano-CaCO3)含量及表面处理对玻璃纤维增强聚苯硫醚(PPS/GF)三元复合材料结晶性能的影响。结果表明:随着Nano-CaCO3质量分数(φf)的增加,经硬脂酸和钛酸酯偶联剂作表面处理的PPS/GF/Nano-CaCO3三元复合体系(SI和SII)的起始结晶温度、结晶温度和结晶度均发生了不同的变化。当φf小于4%时,SII复合体系的结晶度最高。 It studied the influence of the content and surface treatment of Nano-CaCO3 on the crystallization properties of glass fiber-reinforced polyphenylene sulfide(PPSlGF) ternary composites. The results show that the starting crystallization temperature, crystallization temperature and crystalline of PPSlGFINano-CaCO~ composite treated by stearic acid and coupling agent of organic titanate (Sl and Sll)all change with the addition of the particle weigh fraction (φf ). When φf is less than 4%, the crystalline of Sll composite system is the highest.
出处 《塑料科技》 CAS 北大核心 2008年第3期32-35,共4页 Plastics Science and Technology
基金 广东省科技计划项目(No.2004A10702004) 广州市科技攻关项目(No.2004Z3-D2031)
关键词 聚苯硫醚 玻璃纤维 纳米碳酸钙 复合材料 结晶 Polyphenylene sulfide Glass fiber Nano-CaCO3 Composite Crystallization
  • 相关文献

参考文献6

二级参考文献39

共引文献43

同被引文献57

引证文献2

二级引证文献10

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部