摘要
研究了浓硫酸和含硝浓硫酸在80℃和120℃时对316L不锈钢、低铬铸铁、高硅铸铁的腐蚀情况,考察了温度、浓度、应力对腐蚀的影响,对硫酸循环系统设备和管道选材有一定的指导作用。
The corrosion situation of 316L stainless steel, low-chrome cast iron and high-silicon cast iron in oil of vitriol and oil of vitriol containing NO3^- at 80℃ and 120℃ is studied. The influence of temperature, concentration and stress on the corrosion is investigated, which can provide reference to the equipment and pipe materials selecting for sulfuric acid circulating system.
出处
《化学工业与工程技术》
CAS
2008年第1期51-55,共5页
Journal of Chemical Industry & Engineering
关键词
均匀腐蚀
应力腐蚀
含硝浓硫酸
316L不锈钢
低铬铸铁
高硅铸铁
Symmetrical corrosion
Stress corrosion
Oil of vitriol containing NO3
316L stainless steel
Low-chrome castiron
High-silicon cast iron