合成了C11A7·CaCl2和3C2S·3CaSO4·CaF2两种矿物,借助XRD,SEM等测试手段,研究了这二种矿物及其以1∶1掺合时的水化历程。结果表明,矿物3C2S·3CaSO4·CaF2水化能力较弱,但与C11A7·CaCl2共掺时,其水化活性可以大大地得到激发。
In this paper,two minerals C 11 A 7·CaCl 2 and 3C 2S·3CaSO 4·CaF 2 are synthesised.Using XRD,SEM,TGDTA methods,the hydration processes of each of these minerals and mixture of them(each in 50%)are investigated.Results reveal that hydration of 3C 2S·3CaSO 4·CaF 2 is carried out slowly,and can be effectively activated by adding C 11 A 7·CaCl 2.