摘要
应用TEM弱束技术,测得Ll2结构的Ni74.5Pd2Al23.5合金(111)和(100)面的反相畴界APB能分别为(144±20)mJ/m2和(102±11)mJ/m2.实验数据与Ni3Al的APB能数据接近因此,Ni74.5Pd2Al23.
Using the TEM weak beam technigue,the APB energies on the (111) and (100) planes of Ni74.5Pd2A123.5 alloy with L12 structure were determined to be(144±20) mJ / m2 and (102±11) mJ/m2 respectively.The relation of ordering energies on the ductility of the alloy was also discussed in this paper.
出处
《金属学报》
SCIE
EI
CAS
CSCD
北大核心
1997年第11期1130-1134,共5页
Acta Metallurgica Sinica
关键词
镍
铝
钯
金属间化合物
自序能
位错
塑性