摘要 开发了低温液相法—浸取剂TE浸取制备不溶性硫磺新工艺。采用正交试验法得出了低温液相法制备不溶性硫磺粗产品的适宜条件:稳定剂用量0.06%,恒温温度250℃,恒温时间60min,急冷液浓度6.0%。并以单因素法对浸取温度、物料比等浸取工艺参量进行了探讨,其合适条件分别为75~80℃,粗粉料∶浸取剂=1∶(12~15)。在最适宜条件下,产品不溶性硫含量可达92%以上。 Two new processes,low temperature liquid polymerization process and leaching with solvent TE,were developed to produce insoluble sulphur.The optimum production conditions of semifinished product determined by orthogonal design are as follows:stabilizer is 0.06%,temperature is 250℃,reacting time is 60 min and concentration of quenching medium is 6.0% The suitable conditions of leaching process obtained are as follows:temperature is 75~80℃ and ratio of semifinished product to extraction solvent is 1∶12~1∶15 Under the optimum conditions,the content of insoluble sulphur of the product can reach 92%.
出处 《精细化工》 EI CAS CSCD 北大核心 1997年第3期30-32,共3页 Fine Chemicals
关键词 不溶性硫磺 浸取 硫磺 制备 橡胶 硫化剂 insoluble sulphur,low temperature liquid polymerization process,leaching
  • 相关文献

同被引文献148

引证文献32

二级引证文献131

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部