摘要
砷铅锌烧渣与渗透剂一起磨至100%通过-200目后置于搅拌槽中,在选择条件下,用碳浆工艺氰化浸出,可使烧渣中金的含量从7.3g/t下降到0.5~1g/t,具有较好的经济效益。
The roasted residues containing arsenic, lead and zinc were ground with seepage reagent to - 200 mesh( 100% through rate), then sent to a stirring tank. Under the selected condition, the residue was leached with the carbon thick liquid craft cyaniding. The gold content in the residue decreased from 7.3g/t to 0. 5~1g/t. The apply of this technique could obtain good economic efficiency.
出处
《贵金属》
CAS
CSCD
2008年第2期24-27,共4页
Precious Metals
关键词
湿法冶金
砷铅锌烧渣
渗透剂
金
碳浆工艺
hydro- metallurgy
roasted residue containing arsenic, lead and zinc
seepage reagent
gold
carbon thick liquid craft