利用武山铜矿南矿带含铜矽卡岩类型矿石做磨矿介质,成功地实现了南、北矿带混合矿的自磨生产和混合矿浮选,全面优化了选厂的碎磨浮选工艺,缩短了生产流程,流程畅通、生产稳定,并大幅度提高了铜。
Taking Cu bearing skarn ore from the South Belt ore as grinding mediumin autogeneous grinding of mixed ore.This practice completely optimized the comminution and flotation process.The production process is simplified and production is stable.The metallurgical performances of Cu and S have been considerably increased.