摘要 系统研究了添加微量稀土Er对Sn3.8Ag0.7Cu钎料合金显微组织和性能的影响,通过对钎料的熔化温度、润湿性能、接头剪切强度的测试及显微组织观察,指出含微量稀土的SnAgCuEr合金是性能优良的无铅钎料合金,同时确定了最佳的Er含量范围. The effect of minimal amount of rare earth Er on the microstructure and performance of Sn3.8Ag0.7Cu solder alloy, has been systematically investigated. Through measuring the melting temperature, wettability and joint shear strength, and observing the microstructure, it is indicated that the SnAgCuEr alloy containing rare earth is a lead - free solder with an excellent performance. At the same time the best content of Er is de- termined.
出处 《材料科学与工艺》 EI CAS CSCD 北大核心 2008年第2期281-283,共3页 Materials Science and Technology
基金 国家高技术发展计划资助项目(2002AA322040)
关键词 无铅钎料 SnAgCu合金 稀土Er lead- free solder SnAgCu alloy rare earth Er
  • 相关文献

参考文献5

二级参考文献7

  • 1朱颖,方洪渊,钱乙余,丁克俭,薛利忠.Sn-pb-Ce-La钎料合金的显微组织分析[J].稀土,1994,15(1):57-59. 被引量:7
  • 2Richard B. Lead - free soldering - world's apart, National Physical Laboratory[ EB]. NPL News, UK, http://www.lead - free. org, 2004.
  • 3Chen ZG, Shi YW, Xia ZD et al. Properties of leadfree solder SnAgCu containing minute amount of rare earth [J]. Journal of Electronic Materials, 2003, 32 (4) :235 - 243.
  • 4Nimmo K European and international roadmaps for leadfree technology [ EB ]. Soldertee at Tin Technology,UK, http://www. lead - free. org, 2004.
  • 5Porter D A 李长海等(译).金属和合金中的相变[M].北京:冶金工业出版社,1988.354.
  • 6傅高升,孙锋山,任立英,陈文哲,钱匡武.微量稀土对工业纯铝中杂质相的变质行为[J].中国稀土学报,2001,19(2):133-137. 被引量:55
  • 7周守则,陈家应.钇对2024铝合金铸态组织的影响[J].重庆特钢,1992(1):60-64. 被引量:2

共引文献67

同被引文献67

引证文献4

二级引证文献16

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部