1Assad M, Lemieux N, Rivard CH, et al. Comparative in vitro biocompatibility of nickel-titanium, pure nickel, pure titanium,and stainless steel: genotoxicity and atomic absorption evaluation[J]. Biomed Mater Eng, 1999,9: 1.
2Haltia AM, Lahteenkorva K, Tormala P, et al. Self-reinforcement and hydrolytic degradation of amorphous lactic acid based poly (ester-amide), and of its composite with sol-gel derived fibers[J]. J Mater Sci Mater Med, 2002, 13:903.
3Nakafuku C, Takehisa S. Glass transition and mechanical properties of PLLA and PDLLA-PGA copolymer blends[J]. J Appl Polymer Sci, 2004,93 : 2164.
4Jones HP, Lemos MJ, Wilk RM, et al. Two-year follow-up of meniscal repair using a bioabsorbable arrow[J]. Arthroscopy, 2002,18 : 64.
5Tsai AM, McAllister DR, Chow S, et al. Results of meniscal repair using a bioabsorbable screw[J]. Arthroscopy, 2004,20:586.
6Bohnsack M, Borner C, Schmolke S, et al. Clinical results of arthroscopic meniscal repair using biodegradable serews[J].Knee Surg Sports Traumatol Arthrose,2003, 11 :379.
7Willcox N,Roberts S. Delayed biodegradation of a meniscal screw[J]. Arthroscopy, 2004,20 (Suppl 2):20.
8Lembeck B,Wulker N. Severe cartilage damage by broken poly-Llactic acid (PLLA) interference screw after ACL reconstruction[J]. Knee Surg Sports Traumatol Arthrosc, 2005,13 : 283.
9Lajtai G,Schmiedhuber G,Unger F,et al. Bone tunnel remodeling at the site of biodegradable interference screws used for anterior cruciate ligament reconstruction: 5-year follow-up[J]. Arthroscopy ,2001,17 : 597.
10Benedetto KP, Fellinger M,Lim TE,et al. A new bioabsorbable interference screw: preliminary results of a prospective, multicenter, randomized clinical trial[J]. Arthroscopy,2000,16:41.