摘要
系统地进行了标准养护、湿砂养护、保温-标准养护、热水养护四种养护制度对掺偏高岭土活性粉末混凝土强度影响的试验研究。试验结果表明:相同配合比条件下,保温-标准养护混凝土抗压强度最高,湿砂养护次之,标准养护最低;热水养护能加速混凝土强度的发展,特别是前期强度,但后期强度增长有限。
This paper makes a systematic experimental study on the compressive strength of Metakaolin RPC influenced by different curing systems, i.e. standard curing, wet-sand curing, heat preservation-standard curing, and hot water curing. The experiment results show that, under the same mix ratio, heat curing guarantees the highest and quickest compressive strength, followed by wet-sand curing and standard curing; Hot water curing can speed up the strength development of Metakaolin RPC, especially in the initial stage, but the strength development is limited in the later stage.
出处
《石家庄铁道学院学报》
2008年第2期24-27,共4页
Journal of Shijiazhuang Railway Institute
基金
福建省自然科学基金计划资助项目(2007J0163)
福建工程学院科技计划项目(GY-Z0546)
关键词
偏高岭土
活性粉末混凝土
养护制度
强度
metakaolin
reactive powder concrete
curing system
compressive strength