通过改善结合剂的耐火度、流动性、强度,试制用于低温烧成(1000℃以下)的低熔结合剂。该结合剂的强度和制作成的试块的硬度都比较高。
By improving the refi'actoriness, flowability and strength of bonds, we have trial-produecd low-melting bond sample block in low-temperature sintering(under 1000℃).Both the strength of bond and the hardness of sample block produced are appropriate.
出处
《哈尔滨轴承》
2008年第3期27-28,共2页
Journal of Harbin Bearing
关键词
SiC磨具
低温烧成
低熔结合剂
结合剂的强度和硬度
SiC abrasive
low-temperature sintering
low-melting bond
strength and hardness of bond