摘要 通过测定11种不同炼焦煤的煤岩性质和40 kg试验焦炉所炼焦炭抗碎强度分析,确定了基于炼焦煤镜质组最大反射率的活性权函数方程,根据其活性权函数对各炼焦煤的活惰比进行了计算。分析可知,焦炭抗碎强度M_(40)最大时所对应的活惰比为2.17,为优化配煤提供了技术依据。 With the ts on the coal and rock properties of 11 different coking coal and the analysis on the anti-broken strength of coke from the 40 kg test coke oven, The paper had set the activity weight function equation for the max reflection rate based on the vit- finite of the coking coal. According to the activity weight function, the calculation was made on the activity and inert rate of each coking coal. The analysis showed that the anti-broken strength of the coke was M40, the max activity and inert rate was 2. 17, which could provide the technical reference to the optimized coal blending.
出处 《煤炭科学技术》 CAS 北大核心 2008年第9期110-112,共3页 Coal Science and Technology
基金 安徽省科技创新团队资助项目(TD200706)
关键词 煤岩 镜质组平均最大反射率 焦炭抗碎强度 活惰比 试验焦炉 coal and rock average max reflection rate of vitrinite anti-broken strength of coke activity and inert rate test coke oven
  • 相关文献

参考文献3

二级参考文献11

共引文献15

同被引文献76

引证文献10

二级引证文献43

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部