摘要 本文介绍了无收缩高性能混凝土在厦门瑞景公园三期地下室外墙中的应用情况,通过掺入CMA高性能抗裂防水剂适当补偿混凝土早期、中期和后期收缩,克服了掺一般膨胀剂混凝土早期膨胀不明显、中期膨胀太大而后期回缩太大的缺陷,使混凝土适量膨胀、几乎不收缩,解决了地下室外墙混凝土收缩开裂的难题。 It introduces the application of no-shrink high-performance concrete in underground chamber wall in Xiamen Ruijing Park. By adding CMA high-performance anti-crack waterproof admixture to compensate the shrinkage in early, intermediate and final stage, against the defect that the early stage expansion is obscure and the intermediate stage expansion is too large when adding normal expansion admixture, the concrete has properly expansion and no-shrink, solving the difficult about the shrinkage and crack in underground chamber external wall.
作者 吴德立 廖杰
出处 《福建建筑》 2008年第10期58-60,共3页 Fujian Architecture & Construction
关键词 高性能混凝土 CMA高性能抗裂防水剂 膨胀率 回缩量 high-performance concrete CMA high-performance anti-crack waterproof admixture expansion rate shrinkage mass
  • 相关文献

参考文献7

  • 1JGJ55-2000.普通混凝土配合比设计规程[S].[S].,..
  • 2GBJ146-90.粉煤灰混凝土应用技术规程[S].
  • 3GBJ50108-2001,地下工程防水技术规程[S].
  • 4GB50119-2003.混凝土外加剂应用技术规范[S].[S].,..
  • 5GB182-85,普通混凝土长期性能和耐久性能实验方法[S].
  • 6GB/T50080-2002,普通混凝土拌合物性能实验方法标准[S].
  • 7阎培渝 廉慧珍 覃肖.使用膨胀剂配制补偿收缩混凝土时需要注意的几个问题.硅酸盐学报,2000,28:42-45.

共引文献373

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部