3Kim S, Cockcroft S. Mechanical, wear and heat exposure properties of compacted graphite cast iron at elevated temperatures[J]. Journalof Alloys anti Compounds, 2009(487): 253-257.
4Kim S, Cockcroft S. Oplimization of the process pm'ameters 'affecting the microstructures and properties of compacted graphite iron[J]. Journal of Alloys and Compounds, 2009 (476): 728-732.
5Geier G, Bauer W. Micrnstructure transition from lamellar to compaeted graphite using different modification agents[J]. Materials Science and Engineering A, 2005(8).
6Ghaderi A, Ahmadabadi M N. Effect of graphite morphologies on the tribological behavior of auslempered cast iron[J]. Wear, 2003(255).
7Shy Y. Effects of titanium addition and sec.tion size on microstructure and mechanical properties of compacted graphite cast iron[J]. Materials Science and Engineering, 2000(278).