硫酸渣磁选工艺的研究 被引量:2

Study of Magnetic Separation Process for Pyritic Residue
下载PDF
导出
摘要 结合国内硫酸渣应用现状,针对贵州某地硫酸渣的性质和构成特点,采用磁选工艺,使原矿品位由41.89%提高到61.71%,回收率为71.93%,品位提高了近20个品位,硫的含量仅有0.29%;在重磁联合选工艺,精矿的品位达到63.90%,回收率34.51%,中矿品位52.07%,中矿回收率34.08%,硫的含量仅有0.26%,可创造良好的经济效益和环境效益。 Combing the current situation of application of domestic pyritic residue and in the light of the property and constitution characteristics of pyritic residue somewhere in Guizhou Province, magnetic separation process was used to separate the pyritic residue. The results were that the iron grade of the pyritic residue increased nearly 20 percentage points, from 41.89% to 61.71%. The recovery was 71.93 %. The sulfur content was only 0.29%. The results of the combined gravity separation and magnetic separation were that the grade of iron concentrate was 63.90% and the recovery was 34.51%, the grade of middling 52.07% and the recovery 34.08%. The sulfur content was only 0.26%. It achieved better economic and environmental benefits.
出处 《矿业快报》 2008年第10期35-38,共4页 Express Information of Mining Industry
基金 国家教育部项目(Z2005-252003)
关键词 硫酸渣 磁选 铁精矿 Pyritic residue Magnetic separation Iron concentrate
  • 相关文献

参考文献5

二级参考文献30

共引文献23

同被引文献25

引证文献2

二级引证文献9

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部