摘要 造纸碱回收白泥回收窑结圈产生的原因及机理比较复杂,文章分析了白泥及结圈沉积物的化学成分,从原料、燃料及操作参数条件等方面论述了结圈产生的主要原因;探讨了结圈形成及硬化的机理,并介绍了预防及处理结圈的主要措施。 The mechanism and reason of ring formation in lime kiln are complicated. The article analyses the chemical components of the lime mud and the ring deposit. The main factors affecting the ring formation are raw material, fuel and operation parameters, and the main methods for ring prevention and treatment are introduced.
出处 《中国造纸》 CAS 北大核心 2008年第12期58-62,共5页 China Pulp & Paper
关键词 白泥回收窑 白泥 结圈形成及硬化 lime kiln lime mud ring formation and hardening
  • 相关文献

参考文献16

  • 1Efstathios Notidis, Honghi Tran. Survey of lime kiln operation and ringing problems [J]. Tappi Journal, 1993, 76(5): 125
  • 2Barham D, Tran H N. An overview of ring formation in lime kilns [EB/ OL]. Tappi Proceedings, 1990 Pulping Conference, http://www.tappi. org,1990-01-01
  • 3Tran H N , Barham D, Reeve D W. Chloride and Potassium in the Kraft Chemical Recovery Cycle[J]. Pulp & Paper Canada, 1990, 91(5): 185
  • 4Tran H N, Griffiths J, Budge M. Experience of Lime Kiln ringing Problems at E.B Eddy Forest Products[EB/OL].Tappi Journal, 1990 Kraft recovery Operations, http://www.tappi.org, 1990-01-01
  • 5Tran H N. Lime Kiln Chemistry [EB/OL]. Tappi Press 2000, Kraft Recovery Course, http://www.tappi.org ,2000-01-01
  • 6马贤飞.白泥煅烧常见故障及解决办法[J].纸和造纸,2005,24(4):22-24. 被引量:7
  • 7MARIA BJORK. Effects of process variation on ring formation in lime kilns [J]. Tappi Journal, 2005, 4 (6): 20
  • 8彭志坚,陈铁军,胡友明,罗敏,阳仁贵.原料性能对石灰回转窑煅烧及结圈影响的研究[J].钢铁研究,2003,31(3):4-8. 被引量:6
  • 9Notidis E, Tran H N. Survey of Ring Formation in Lime Kilns [EB/ OL]. Tappi Journal, 1992 Pulping Conference, http: //www.tappi. org, 1992-01-01
  • 10Ellis K. Ring formation in a NCG burning lime kiln [C]. Proc.1989 Tappi Environ Conference, Tappi Press, 1989

共引文献11

同被引文献52

引证文献1

二级引证文献1

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部