通过对钛白粉成品筛余物偏高的原因进行分析,有针对性地从生产设备和工艺两个方面进行改进,使钛白粉成品细度指标由改进前的0.05%~0.1%降低到改进后0.05%以下,达到国内优等品的细度要求。
The problem of residue on sieve of titanium pigment is high was analyzed. The equipments and technics were improved. The fineness of titanium pigment lowered to 0.05% below from 0.05% -0.1%, which meets the requirement of high - class products.