摘要 为保证某型直升机延寿后的飞行安全,对其疲劳危险部位根部接头进行了材料断裂性能试验,并对试验数据进行分析处理。通过计算,对比研究了不同裂纹扩展公式下的裂纹扩展寿命。采用考虑因素较全面的,且具有较高可靠度的全范围Forman公式进行裂纹扩展寿命分析,得到不同风险率下的裂纹扩展寿命,并给出了适合的检查周期。 In order to guarantee the fly safety of certain helicopter's main blade after prolonging life, the material's rupture performance test was carried on the fatigue danger parts of the helicopter's root tie-in, and then the test data were analyzed and disposed. Through calculation, different crack growth lives among different crack growth formulas were contrasted. Then the crack growth lives were analyzed with the crack growth formula of full range Forman formula with reliabilities, and the inspection periods were given.
出处 《无损检测》 2009年第3期188-191,共4页 Nondestructive Testing
关键词 裂纹扩展模型 断裂性能试验 可靠度 裂纹扩展寿命 检查周期 Crack growth model Rupture performance test Reliability Crack growth life Inspection period
  • 相关文献

参考文献7

  • 1李庆芬,胡胜海,朱世范.断裂力学及其工程应用[M].哈尔滨:哈尔滨工程大学出版社,2005.
  • 2.某型直升机动部件延寿技术[R]:中国海军科技报告.青岛,2003..
  • 3穆志韬,华然,段成美.高周疲劳载荷环境下直升机动部件的损伤容限分析[J].机械强度,2002,24(1):113-115. 被引量:13
  • 4刘文廷,断裂性能测试[M].北京:北京航空航天大学出版社,1985.
  • 5陈瑞峰,陈浩然,任明法,何宇廷,傅祥炯.裂纹扩展寿命模型的对比研究[J].计算力学学报,1997,14(2):236-240. 被引量:3
  • 6熊峻江 高镇同.广义断裂等寿命曲线与二维门槛值概率分布.北京航空航天大学学报,2000,13(2):206-211.
  • 7王永廉 吴永瑞.一个适用性广泛的疲劳裂纹扩展速率表达式 [J].航空学报,1987,8(4):191-196.

二级参考文献7

  • 1-.美国空军损伤容限手册[M].西安:西北工业大学出版社,1989..
  • 2陈瑞峰,大连理工大学学报,1997年
  • 3傅祥炯,Eng Fract Mech,1989年,34卷,1241页
  • 4团体著者,随机载荷谱裂纹扩展寿命模型,1989年
  • 5Chang J B,ASTM STP 748,1981年
  • 6吴学仁.飞机结构金属材料力学性能手册[M].北京:航空工业出版社,1998.238-239.
  • 7吴学仁.飞机结构金属材料力学性能手册[M].北京:航空工业出版社,1996..