摘要
针对该选厂以往-0.5 mm细泥锰矿直接抛尾,在查明矿石性质的基础上,采用单一磁选流程,可以获得较好的技术指标。在原矿品位为13.3%;锰回收率为40%;精矿品位可达到25%。为-0.5 mm细泥锰矿回收找到切实可行的方法。
In view of the plant before the election - 0.5 mm of thin manganese direct in throwing mud tail,in identifying the nature of ore on the basis of a single magnetic separation process, we have got better technical indicators. In ore grade of 13.3%, manganese recovery was 40% and concentrate grade could reach 25%. -0.5 mm of thin soil manganese recovery has found a realistic and practical approach.
出处
《中国锰业》
2009年第1期32-34,共3页
China Manganese Industry
关键词
锰矿
磁选
提高回收率
Manganese
Magnetic
Increase in the recovery rate