摘要
Φ8~Φ12是45钢的水淬淬裂危险尺寸。通过对具有淬裂危险尺寸45钢小工件的工艺改进,探讨了亚温淬火的作用机理。
45# steel with Φ8~Φ 12 diameter is the possible quench crack size in water quench- Based on quench technique improvement on 45# steel small elements being of possible quench crack s1ze,the mechanlsm of subnormal temperature quench is discussed.
出处
《石家庄铁道大学学报(自然科学版)》
1998年第S1期86-88,共3页
Journal of Shijiazhuang Tiedao University(Natural Science Edition)
关键词
45钢工件
淬裂危险尺寸
亚温淬火
45~# steel element
possible quench crack size
subnormal temperature quench